Chrome Plated Round Bars

Test Reports available on request

C1045/C1050

Chemistry   Yield Chrome Hardness Elongation Surface 
    PSI in 2" Min Finish
Carbon 0.43 - 0.50 50K Re 67-72 40% Ra-16 Max
Manganese 0.60 - 0.90 75K Re 67-72 35% Ra-16 Max
Phosphorus .040 Max. 100K Re 67-72 32% Ra-16 Max
Sulphur .050 Max        
Plate Thickness   .0005" min    
    0.001" min    
Salt Spray Test   48 hrs min. meets ASTM B-1117